Crystal specification:  
Plant Number (Serial): 4899
Type: 2 L
   
Data from BTCP:  
Length: 199.982 mm
Dimensions front: AF: 21.118 mm, BF3: 21.24 mm, BF4: 21.25 mm, CF: 21.325 mm
Dimensions back: AR: 28.723 mm, BR3: 28.696 mm, BR4: 28.71 mm, CR: 29.003 mm
Transmittance: 49.4 % at λ = 360 nm, 72.6 % at λ = 420 nm, 76.3 % at λ = 620 nm
Light yield: 21.5
ΔK: 0.827 m-1
Spread for T = 50 %: 0.4 nm
Lot: B-10
ACCOS machine: 3
Specification passed: Yes
   
Data from CERN:  
Length: 200.004 mm
Dimensions front: AF: 21.019 mm, BF3: 21.247 mm, BF4: 21.23 mm, CF: 21.227 mm
Dimensions back: AR: 28.655 mm, BR3: 28.719 mm, BR4: 28.694 mm, CR: 28.936 mm
Transmittance: 45.4 % at λ = 360 nm, 69.3 % at λ = 420 nm, 74 % at λ = 620 nm
Light yield: 24.9145
Light yield coefficient: 0.374091
Spread for T = 50 %: 2.03 nm
Lot: B-10
ACCOS machine: 1
Specification passed: Yes
   
Data from JLU Gießen:  
Transmittance: 0 % at λ = 360 nm, 0 % at λ = 420 nm, 0 % at λ = 620 nm
Transmittance AI: 0 % at λ = 360 nm, 0 % at λ = 420 nm, 0 % at λ = 620 nm
Time AI: 0
Light yield: 0
ΔK: 0 m-1
Box Number: 0
Lot:
Specification passed: No
Comments:
   
Crystal State:  
Broken?: No
Location: unknown
Location Details: unknown
Notes:


Version history

Time Author Change comment
21. Apr 2017 13:17:54 CEST Tobias Imported crystal from database at JLU Gießen