Crystal specification:  
Plant Number (Serial): 3706
Type: 3 R
   
Data from BTCP:  
Length: 199.946 mm
Dimensions front: AF: 21.109 mm, BF3: 21.251 mm, BF4: 21.209 mm, CF: 21.449 mm
Dimensions back: AR: 28.324 mm, BR3: 28.733 mm, BR4: 28.678 mm, CR: 28.784 mm
Transmittance: 50.6 % at λ = 360 nm, 71.9 % at λ = 420 nm, 75.6 % at λ = 620 nm
Light yield: 19
ΔK: 0.903 m-1
Spread for T = 50 %: 0.43 nm
Lot: B-10
ACCOS machine: 3
Specification passed: Yes
   
Data from CERN:  
Length: 199.987 mm
Dimensions front: AF: 21.014 mm, BF3: 21.252 mm, BF4: 21.204 mm, CF: 21.347 mm
Dimensions back: AR: 28.234 mm, BR3: 28.745 mm, BR4: 28.682 mm, CR: 28.685 mm
Transmittance: 48 % at λ = 360 nm, 70.9 % at λ = 420 nm, 74.9 % at λ = 620 nm
Light yield: 26.2511
Light yield coefficient: 0.394161
Spread for T = 50 %: 0.6 nm
Lot: B-10
ACCOS machine: 1
Specification passed: Yes
   
Data from JLU Gießen:  
Transmittance: 0 % at λ = 360 nm, 0 % at λ = 420 nm, 0 % at λ = 620 nm
Transmittance AI: 0 % at λ = 360 nm, 0 % at λ = 420 nm, 0 % at λ = 620 nm
Time AI: 0
Light yield: 0
ΔK: 0 m-1
Box Number: 0
Lot:
Specification passed: No
Comments:
   
Crystal State:  
Broken?: No
Location: unknown
Location Details: unknown